News classification
Technical index of fine veneer rubber
Time:2018-10-30 08:48:51 Page view (895)
Technical index of fine veneer rubber
Technical indicators appearance white liquid
The solid content is 90 or more than 50%.
Viscosity 90000-100000, MPA.S (25 C)
PH 5-7
A wood rubber
For 200 wire -300 wire veneer, cold and hot press.
The solid content is 90 or more than 35%.
Viscosity 50000-60000, MPA.S (25 C)
PH 4-6
C wood rubber
For 100 wire -50 wire veneer veneer.
The solid content is 90 or more than 30%.
Viscosity 45000-50000, MPA.S (25 C)
PH 4-6
Instructions:
1, the surface of the sheet should be smooth and smooth, and the wood skin must be free from dust and cracking.
2, wood skin is not smooth or radiant material, must be double-sided glue.
3, the temperature of the electric iron should be between 100 -200 and C. the electric iron must be clean and smooth.
4. The best use of wool roller is to ensure that the fabric is evenly distributed. No use of brush or chopper.
5. The double-sided cloth glue is first coated with wood skin and then with base material. After the wood skin is half-dry, the wood skin is glued on and heated with an iron.
6. One-sided cloth glue, first coat glue, a large amount of glue, before the glue is dry, stick the wooden skin, hand to flatten the wooden skin, so that the glue watermarking on the wooden skin, electric iron heating can be pushed dry.
Technical indicators appearance white liquid
The solid content is 90 or more than 50%.
Viscosity 90000-100000, MPA.S (25 C)
PH 5-7
A wood rubber
For 200 wire -300 wire veneer, cold and hot press.
The solid content is 90 or more than 35%.
Viscosity 50000-60000, MPA.S (25 C)
PH 4-6
C wood rubber
For 100 wire -50 wire veneer veneer.
The solid content is 90 or more than 30%.
Viscosity 45000-50000, MPA.S (25 C)
PH 4-6
Instructions:
1, the surface of the sheet should be smooth and smooth, and the wood skin must be free from dust and cracking.
2, wood skin is not smooth or radiant material, must be double-sided glue.
3, the temperature of the electric iron should be between 100 -200 and C. the electric iron must be clean and smooth.
4. The best use of wool roller is to ensure that the fabric is evenly distributed. No use of brush or chopper.
5. The double-sided cloth glue is first coated with wood skin and then with base material. After the wood skin is half-dry, the wood skin is glued on and heated with an iron.
6. One-sided cloth glue, first coat glue, a large amount of glue, before the glue is dry, stick the wooden skin, hand to flatten the wooden skin, so that the glue watermarking on the wooden skin, electric iron heating can be pushed dry.