Hot pressing adhesive precautions
Time:2019-05-27 12:21:35 Page view (833)
Hot pressing adhesive precautions
Hot pressing adhesive precautions
Two or more monomers of PVAC and BA are copolymerized.
(1) The temperature and the amount of glue applied can be based on the environment and the "viscosity" of the glue and the thickness of the veneer.
(2) The two components can be determined according to the water resistance requirements of your product and the performance of mechanical equipment.
(4) (3) If your product is a concave-convex type, it is recommended to use a rubber waterbed type heating press; if it is a flat iron plate press, it is recommended to add a padding (thickness 3mm) when your product is pressed. In order to ease the borrowing power, it does not blister and does not penetrate the glue.
(4) The magnitude of the pressure, the temperature and the length of the pressing time are determined by the thickness of the veneer material.
(5) Use temperature (cold pressure) of 10 ° C or more.
Shanghai Zhenniu Chemical Co., Ltd.
Hot pressing adhesive precautions
Two or more monomers of PVAC and BA are copolymerized.
(1) The temperature and the amount of glue applied can be based on the environment and the "viscosity" of the glue and the thickness of the veneer.
(2) The two components can be determined according to the water resistance requirements of your product and the performance of mechanical equipment.
(4) (3) If your product is a concave-convex type, it is recommended to use a rubber waterbed type heating press; if it is a flat iron plate press, it is recommended to add a padding (thickness 3mm) when your product is pressed. In order to ease the borrowing power, it does not blister and does not penetrate the glue.
(4) The magnitude of the pressure, the temperature and the length of the pressing time are determined by the thickness of the veneer material.
(5) Use temperature (cold pressure) of 10 ° C or more.