News classification
Technical parameters of woodworking glue
Time:2019-03-28 09:53:53 Page view (776)
Technical parameters of woodworking glue
Technical parameters of woodworking glue:
Appearance: Milky white viscous liquid Solid content: 26±1% (105°C, 3h) PH value: 3.0~5.0
Surface bonding strength: >0.5Mpa
Theoretical coating amount: Panels with a coating area of 3.5 to 5.0 square meters per liter. Due to the different surface roughness of the wood, the amount of glue consumed will increase or decrease.
Instructions for use:
1. This product is a special glue for wood products bonding. It is suitable for veneer bonding of woodwork products such as home decoration and tooling.
2. After the lid is opened, stir it evenly, and apply the glue to the one or both sides of the material to be bonded. The amount of glue applied should not be discharged after bonding.
3. After bonding, it needs to be evenly pressurized (it can also be pressurized by rivet). The pressing time should not be lower than 24 hours. After the pressing, it can be laid for 96 hours before cutting can be done. 12 days). Adhesive pressurization time is greatly affected by temperature and humidity, and it is necessary to prolong the pressurization and dispersing time in a low temperature or humid environment.
4, can not pressurize and can not be rivets, try to close the panel and the bottom plate for a fixed period of time, after the glue is dry and solid.
Technical parameters of woodworking glue:
Appearance: Milky white viscous liquid Solid content: 26±1% (105°C, 3h) PH value: 3.0~5.0
Surface bonding strength: >0.5Mpa
Theoretical coating amount: Panels with a coating area of 3.5 to 5.0 square meters per liter. Due to the different surface roughness of the wood, the amount of glue consumed will increase or decrease.
Instructions for use:
1. This product is a special glue for wood products bonding. It is suitable for veneer bonding of woodwork products such as home decoration and tooling.
2. After the lid is opened, stir it evenly, and apply the glue to the one or both sides of the material to be bonded. The amount of glue applied should not be discharged after bonding.
3. After bonding, it needs to be evenly pressurized (it can also be pressurized by rivet). The pressing time should not be lower than 24 hours. After the pressing, it can be laid for 96 hours before cutting can be done. 12 days). Adhesive pressurization time is greatly affected by temperature and humidity, and it is necessary to prolong the pressurization and dispersing time in a low temperature or humid environment.
4, can not pressurize and can not be rivets, try to close the panel and the bottom plate for a fixed period of time, after the glue is dry and solid.